ملخص
The corrosion behavior of α-Al-bronze (Cu-7%A1) was studied in 3.4% NaCl solution for extended periods of time using x-ray diffraction, x-ray photoelectron spectroscopy, optical and scanning electron microscopy, and electrochemical polarization measurements. Corrosive attack occurs very early leading to general corrosion and pit nucleation, coalescence, growth, and eventual merging of neighboring pits together to give multiple trough-like cavities. The corrosion products which form under free corrosion conditions appear as a duplex film with an inner adherent layer of A12O3 and an outer layer of Cu2O, cu2(OH)3C1, and Cu(OH)Cl. The x-ray measurements revealed several significant findings: (i) the Cu(111) plane corrodes preferentially, (ii) Cu2O forms very early under open-circuit conditions and grows progressively with time. Conversely Cu(OH)Cl was detected microscopically on the corroded surface after 9 days and by x-ray diffraction after much longer times, (iii) CuCl forms only at anodic potentials, considerably higher than the free corrosion potential. Indeed, it was not detected under free corrosion conditions, and (iv) the composition of the corrosion products which were retained on the alloy surface is quite different from those which spalled off the corroding surface.
| اللغة الأصلية | English |
|---|---|
| الصفحات (من إلى) | 71-78 |
| عدد الصفحات | 8 |
| دورية | Journal of the Electrochemical Society |
| مستوى الصوت | 141 |
| رقم الإصدار | 1 |
| المعرِّفات الرقمية للأشياء | |
| حالة النشر | Published - يناير 1994 |
| منشور خارجيًا | نعم |
بصمة
أدرس بدقة موضوعات البحث “Corrosion of α-Al Bronze in Saline Water'. فهما يشكلان معًا بصمة فريدة.قم بذكر هذا
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver