Nanoindentation of wet and dry compact bone: Influence of environment and indenter tip geometry on the indentation modulus

  • G. Guidoni*
  • , M. Swain
  • , I. Jäger
  • *المؤلف المقابل لهذا العمل
  • University of Leoben
  • Biomaterials Science Research Unit
  • The University of Sydney
  • Department of Materials Physics

نتاج البحث: Article › مراجعة النظراء

40 اقتباسات (Scopus)

ملخص

The indentation-derived elastic modulus, E, of bovine compact bone was obtained by nanoindentation. The indentation modulus of the dry condition (i.e. under atmospheric conditions) is 40% higher than when measured wet (i.e. immersed in buffer solution). Although this difference is independent of orientation, there is a 20% difference in the indentation modulus within the same tested environment between longitudinal and transversal directions. In addition, the estimated indentation modulus of the same samples when tested wet in buffer solution after deep freezing (-15°C) was not affected. The discrepancy between wet and dry results was attributed to the non-mineralized phase contribution and rationalized by a simple mechanical model [I. Jager and P. Fratzl, Biophys. J. 79 (2000) p.1737]. Anisotropy effects could be explained in terms of deformation mechanisms with orientation. The effect of frozen storage temperatures may be clarified considering the biomechanics of the helicoidal arrangement of lamellar bone. Viscoelastic effects were also considered and incorporated into analysis of the force-displacement data.

اللغة الأصليةEnglish
الصفحات (من إلى)553-565
عدد الصفحات13
دوريةPhilosophical Magazine
مستوى الصوت90
رقم الإصدار5
المعرِّفات الرقمية للأشياء
حالة النشرPublished - فبراير 2010
منشور خارجيًانعم

بصمة

أدرس بدقة موضوعات البحث “Nanoindentation of wet and dry compact bone: Influence of environment and indenter tip geometry on the indentation modulus'. فهما يشكلان معًا بصمة فريدة.

قم بذكر هذا