تخطي إلى التنقل الرئيسي تخطي إلى البحث تخطي إلى المحتوى الرئيسي

Stress corrosion behavior of α-aluminum bronze in saline water

  • B. G. Ateya*
  • , E. A. Ashour
  • , S. M. Sayed
  • *المؤلف المقابل لهذا العمل
  • Cairo University

نتاج البحث: Article

42 اقتباسات (Scopus)

ملخص

α-Aluminum bronze (Copper [Cu]-7% Al) (UNS C61400) was found to be susceptible to stress corrosion cracking (SCC) in 3.4% NaCl under relatively high anodic potentials (≥300 mVNHE), i.e., greater than 200 mV more positive than the free-corrosion potential. The time to failure and stress ratio (σ soln/σ air) were mildly dependent on potential. The fracture mode changed from ductile under open-circuit and mild anodic or cathodic potentials to brittle at 300 mVNHE. Electrochemical and x-ray diffraction data were obtained to suggest interpretations for the SCC measurements. The bronze's susceptibility to SCC at high anodic potentials was attributed to the presence of cuprous chloride (CuCl) on the surface. CuCl was absent at low potentials. The bronze's resistance to SCC at low potentials was attributed to the presence of θ-aluminum oxide, which was detected by x-ray diffraction on the corroded surface.

اللغة الأصليةEnglish
الصفحات20-25
عدد الصفحات6
مستوى الصوت50
رقم1
منشور متخصصCorrosion
المعرِّفات الرقمية للأشياء
حالة النشرPublished - 1994
منشور خارجيًانعم

بصمة

أدرس بدقة موضوعات البحث “Stress corrosion behavior of α-aluminum bronze in saline water'. فهما يشكلان معًا بصمة فريدة.

قم بذكر هذا