Comparison of three and four point bending evaluation of two adhesive bonding systems for glass-ceramic zirconia bi-layered ceramics

  • C. Gee
  • , J. N. Weddell
  • , M. V. Swain*
  • *Corresponding author for this work
  • University of Otago

Research output: Contribution to journal › Article › peer-review

20 Scopus citations

Abstract

Objectives To quantify the adhesion of two bonding approaches of zirconia to more aesthetic glass-ceramic materials using the Schwickerath (ISO 9693-2:2016) three point bend (3PB) [1] test to determine the fracture initiation strength and strain energy release rate associated with stable crack extension with this test and the Charalamabides et al. (1989) [2] four point bend (4PB) test. Methods Two glass-ceramic materials (VITABLOCS Triluxe forte, Vita Zahnfabrik, Germany and IPS.emax CAD, Ivoclar Vivadent, Liechtenstein) were bonded to sintered zirconia (VITA InCeram YZ). The former was resin bonded using a dual-cure composite resin (Panavia F 2.0, Kuraray Medical Inc., Osaka, Japan) following etching and silane conditioning, while the IPS.emax CAD was glass bonded (IPS e.max CAD Crystall/Connect) during crystallization of the IPS.emax CAD. Specimens (30) of the appropriate dimensions were fabricated for the Schwickerath 3PB and 4PB tests. Strength values were determined from crack initiation while strain energy release rate values were determined from the minima in the force-displacement curves with the 3PB test (Schneider and Swain, 2015) [3] and for 4PB test from the plateau region of stable crack extension. Results Strength values for the resin and glass bonded glass ceramics to zirconia were 22.20 ± 6.72 MPa and 27.02 ± 3.49 MPa respectively. The strain energy release rates for the two methods used were very similar and for the glass bonding, (4PB) 15.14 ± 5.06 N/m (or J/m2) and (3PB) 16.83 ± 3.91 N/m and resin bonding (4PB) 8.34 ± 1.93 N/m and (3PB) 8.44 ± 2.81 N/m respectively. The differences in strength and strain energy release rate for the two bonding approaches were statistically significant (p < 0.05). SEM observations showed fracture occurred adhesively for the resin bonding and cohesively for the glass bonding. Significance The present results indicate 3PB and 4PB tests have very similar values for the strain energy release rate determination. However while strength tests reveal minimal differences between resin and glass bonding, strain energy release rates for the latter are superior for bonding CAD/CAM milled glass-ceramics to zirconia.

Original languageEnglish
Pages (from-to)1004-1011
Number of pages8
JournalDental Materials
Volume33
Issue number9
DOIs
StatePublished - Sep 2017

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 7 - Affordable and Clean Energy
    SDG 7 Affordable and Clean Energy
  2. SDG 9 - Industry, Innovation, and Infrastructure
    SDG 9 Industry, Innovation, and Infrastructure
  3. SDG 12 - Responsible Consumption and Production
    SDG 12 Responsible Consumption and Production

Keywords

  • Adhesion
  • Composite resin bonding
  • Four-point bend testing
  • Glass bonding
  • Glass-ceramic
  • Schwickerath testing
  • Strain energy release rate
  • Zirconia

Fingerprint

Dive into the research topics of 'Comparison of three and four point bending evaluation of two adhesive bonding systems for glass-ceramic zirconia bi-layered ceramics'. Together they form a unique fingerprint.

Cite this