Abstract
α-Aluminum bronze (Copper [Cu]-7% Al) (UNS C61400) was found to be susceptible to stress corrosion cracking (SCC) in 3.4% NaCl under relatively high anodic potentials (≥300 mVNHE), i.e., greater than 200 mV more positive than the free-corrosion potential. The time to failure and stress ratio (σ soln/σ air) were mildly dependent on potential. The fracture mode changed from ductile under open-circuit and mild anodic or cathodic potentials to brittle at 300 mVNHE. Electrochemical and x-ray diffraction data were obtained to suggest interpretations for the SCC measurements. The bronze's susceptibility to SCC at high anodic potentials was attributed to the presence of cuprous chloride (CuCl) on the surface. CuCl was absent at low potentials. The bronze's resistance to SCC at low potentials was attributed to the presence of θ-aluminum oxide, which was detected by x-ray diffraction on the corroded surface.
| Original language | English |
|---|---|
| Pages | 20-25 |
| Number of pages | 6 |
| Volume | 50 |
| No | 1 |
| Specialist publication | Corrosion |
| DOIs | |
| State | Published - 1994 |
| Externally published | Yes |
Fingerprint
Dive into the research topics of 'Stress corrosion behavior of α-aluminum bronze in saline water'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver