Stress corrosion behavior of alpha aluminum bronze in concentrated alkali solutions

  • E. A. Ashour*
  • , E. A.A. El Meguid
  • , B. G. Ateya
  • *Corresponding author for this work
  • Physical Chemistry Department
  • National Research Center

Research output: Contribution to journal › Article › peer-review

6 Scopus citations

Abstract

Stress corrosion behavior of alpha Al bronze (Cu-7%Al) (UNS C6 1400) was studied in solutions of 0.1 M to 8 M sodium hydroxide (NaOH) under various potentials (-600 mV vs normal hydrogen electrode NHE to 800 mVNHE) and slow strain rates. Analysis of the results of time-to-failure (tf). maximum yield stress (σmax), and the morphology of the fracture surface indicates that the alloy resists stress corrosion cracking (SCC) under all test conditions, including those where the alloy undergoes selective dissolution. The susceptibility (S) to SCC in the above tests was ≤ 14% where S combines the ratios of tf and σmax under the test and in air.

Original languageEnglish
Pages (from-to)749-752
Number of pages4
JournalCorrosion
Volume57
Issue number9
DOIs
StatePublished - 2001
Externally publishedYes

Keywords

  • Aluminum bronze
  • Caustic alkali
  • Cooper
  • Selective dissolution
  • Stress corrosion cracking

Fingerprint

Dive into the research topics of 'Stress corrosion behavior of alpha aluminum bronze in concentrated alkali solutions'. Together they form a unique fingerprint.

Cite this